Dear All,
Thanks for all response to my previous thread although I feel sad about the funny thread. I believe you all have missunderstood for what I asked for.
I have another problem to be discussed. I have my steam line which has been experienced corroded problem frequently. If I partially replace the existing carbon steel line with stainless pipe (especially for the vertical line), what would be happened related to thermal expansion. I have calculated the delta length as the result of expanded stainless pipe. I cannot add any expansion belows or expansion bent on that line to absorb the expansion due to limited space. Do you guys have any idea..?? (hope this thread is not funny)
regards.
Thanks for all response to my previous thread although I feel sad about the funny thread. I believe you all have missunderstood for what I asked for.
I have another problem to be discussed. I have my steam line which has been experienced corroded problem frequently. If I partially replace the existing carbon steel line with stainless pipe (especially for the vertical line), what would be happened related to thermal expansion. I have calculated the delta length as the result of expanded stainless pipe. I cannot add any expansion belows or expansion bent on that line to absorb the expansion due to limited space. Do you guys have any idea..?? (hope this thread is not funny)
regards.