I have an ancient part in our system that needs to be produced.
On the dwg, it says, "Steam Homo Draw at 650F, dip in oil".
The material is 1144 steel.
My limited Google search says this process to be
some sort of proprietary process for corrosion protection...like passivation?
Anyway..what exactly is this process?
None of my 2 heat treaters know what this is....or have heard of it.
Is there an equivalent process...black oxide maybe?
Thanks in advance.
On the dwg, it says, "Steam Homo Draw at 650F, dip in oil".
The material is 1144 steel.
My limited Google search says this process to be
some sort of proprietary process for corrosion protection...like passivation?
Anyway..what exactly is this process?
None of my 2 heat treaters know what this is....or have heard of it.
Is there an equivalent process...black oxide maybe?
Thanks in advance.