Attempting to locate supplier of Stainless Steel X17CrNi 16-2, QT800 in 3.75” Dia. Bar. Can you assist? Thank you.
 
Replies continue below

Recommended for you

have you got a UNS number for that alloy?

= = = = = = = = = = = = = = = = = = = =
Plymouth Tube
 
Checking ASM's Worldwide Guide to Equivalent Irons and Steels, 3rd Ed., shows that X17CrNi16-2 falls into the UNS S43100, AISI 431, and EN10088-3 categories. Check with your suppliers to see if they can supply their S43100/AISI 431 material to meet your specific requirements of X17CrNi16-2.

X17CrNi16-2 is an Italian specification. A quick internet search provided 2 good references for equivalents:



Good Luck
 
Thank you for opening up what had been a dead end for me on this so far. Really appreciate your efforts.
 
The one thing that you will need to double check is the carbon level. This alloy is made with a number of different carbon levels for different applications.

= = = = = = = = = = = = = = = = = = = =
Plymouth Tube
 