Stainless Steel Welding without Back Purging

Status
Not open for further replies.

uglyspec

Mechanical
Dec 31, 2013
41
If I back weld a stainless steel joint butt joint with FCAW would I then need to grind, gouge and clean up the opposite side prior to welding? Or should back welding limit the oxidation and sugaring?

Thanks!
 
Replies continue below

Recommended for you

Absolutely you need to remove the heat tint/oxidation from back welding with no purge and prepare the opposite side of the weld prep for welding.
 