I would appreciate an advice on the subject. i have thick Wall Filters (2" thick) having design temperature and pressure as 250 Deg F and 890 psig. Since, the thickness of the vessel qualifies the same to be subjected to PWHT as per code requirements same would be performed. But, the catch is these filters have tube sheets that bear the metallurgy as SS 304 which needs to be welded to these shell.
Question is how would the welding of SS tube sheet be performed on the vessel which has to undergo PWHT?
Letting the SS tube sheet inside shell will subject the same for sensitization.
Can you please advise what shall be the procedure to perform the same. These tube sheets are close tolerance with shell so buttering may cause fitment issues for tube sheets.
Can someone please advise?
Question is how would the welding of SS tube sheet be performed on the vessel which has to undergo PWHT?
Letting the SS tube sheet inside shell will subject the same for sensitization.
Can you please advise what shall be the procedure to perform the same. These tube sheets are close tolerance with shell so buttering may cause fitment issues for tube sheets.
Can someone please advise?