Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations MintJulep on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

stainless steel melting prodceedure 4

Status
Not open for further replies.

ornamentalbob

Mechanical
Joined
Mar 21, 2005
Messages
1
Location
GB
i am soon to start melting stainless steel in a 100kg induction furnace and pouring the metal into lost wax process moulds any advice in melting proceedure and moulding proceedure would be most welcome
 
ornamentalbob

In case you were not aware of it, there is a relativley new forum dedicated to this subject:

forum1135 - The forum's goal is to address any and all questions regarding stainless steel. It will help form the content of an upcoming book on stainless steel.

 
use clean and dry scrap. I suppose you have basic lining in te furnace. keep the melt covered and do not stir frequently. Add your alloys like LC FeCr, LC FeMn, FeSi just before tapping. If possible pass Argon gas. Add very small quantities of Se powder(20gms for 50 kgs) and CaSi to the stream while tapping.


With these few steps you should get a good metal poured into the shell.
 