Can someone suggest a stainless steel that can be hardened to 55 RC and has good impact toughness?

Corrosion resistance is really not an issue as I am only considering stainless as a replacement for low alloy carbon steel because stainless responds better to a nitriding process I am considering.

Thanks in advance.

Bill
 
Replies continue below

Recommended for you

The classic grade for this is 420. There are several much more expensive grades which are sometimes used for knife blades, which engineers at Crucible or Timken/Latrobe could help you with.
 