Jan 30, 2006 #1 arunmrao Materials Joined Oct 1, 2000 Messages 4,758 Location IN I have just received a mail mentioning that furnace liners casting grade HK for copper smelter are failing early. Please suggest if anyone has any experience in this area. Will be most grateful for any assistance.
I have just received a mail mentioning that furnace liners casting grade HK for copper smelter are failing early. Please suggest if anyone has any experience in this area. Will be most grateful for any assistance.
Jan 31, 2006 Thread starter #2 arunmrao Materials Joined Oct 1, 2000 Messages 4,758 Location IN C 0,4-0,6; Cr 35-37; Ni 45-48; Si 1-2; Nb 0,8-1,2; Mo 0,5-0,8; Ti 0,5-0,8; This is the alloy which my good friends from AFE Klefisch have recommended. The cost is going to be prohibitive I suppose for replacement Upvote 0 Downvote