Sep 6, 2012 #1 dharr25301 Mechanical Joined Jul 27, 2012 Messages 9 Location GB Hi, Can anyone advise as to what the minimum Yield is for stainlees steel 316L? Many Thanks, Dave.
Sep 6, 2012 1 #2 arunmrao Materials Joined Oct 1, 2000 Messages 4,758 Location IN Refer Metals Handbook or do a Google search. _____________________________________ "It's better to die standing than live your whole life on the knees" by Peter Mayle in his book A Good Year Upvote 0 Downvote
Refer Metals Handbook or do a Google search. _____________________________________ "It's better to die standing than live your whole life on the knees" by Peter Mayle in his book A Good Year
Sep 6, 2012 1 #3 TVP Materials Joined Apr 12, 2002 Messages 4,592 Location US It will depend on the product form, industry specification, etc. The following datasheet shows typical properties for rolled sheet: http://www.aksteel.com/pdf/markets_products/stainless/austenitic/316_316L_Data_Bulletin.pdf Upvote 0 Downvote
It will depend on the product form, industry specification, etc. The following datasheet shows typical properties for rolled sheet: http://www.aksteel.com/pdf/markets_products/stainless/austenitic/316_316L_Data_Bulletin.pdf
Sep 7, 2012 Thread starter #4 dharr25301 Mechanical Joined Jul 27, 2012 Messages 9 Location GB Thanks Armunmrao, i already googled and i got 170Mpa. However being a novice i wasn't confident it was the right answer. TVP - thanks for the PDF, very useful.. Upvote 0 Downvote
Thanks Armunmrao, i already googled and i got 170Mpa. However being a novice i wasn't confident it was the right answer. TVP - thanks for the PDF, very useful..
Sep 7, 2012 1 #5 EdStainless Materials Joined May 20, 2004 Messages 16,369 Location Waukesha WI USA In ASTM specs it is listed as 25ksi (170MPa) with a UTS or 70ksi (485MPa) = = = = = = = = = = = = = = = = = = = = Plymouth Tube Upvote 0 Downvote
In ASTM specs it is listed as 25ksi (170MPa) with a UTS or 70ksi (485MPa) = = = = = = = = = = = = = = = = = = = = Plymouth Tube