Jul 15, 2015 #1 pperlich Mechanical Joined Jun 17, 2014 Messages 128 Location US Is it permissible to use F563C, F593D, F593G, and F593H bolts in a Div.1 PV? Thanks!
Jul 18, 2015 #2 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US What are these designations? Upvote 0 Downvote
Jul 21, 2015 Thread starter #3 pperlich Mechanical Joined Jun 17, 2014 Messages 128 Location US ASTM F593 http://www.portlandbolt.com/technical/specifications/astm-f593/ I would say they are not permitted in a Div. 1 PV. Is that correct? Upvote 0 Downvote
ASTM F593 http://www.portlandbolt.com/technical/specifications/astm-f593/ I would say they are not permitted in a Div. 1 PV. Is that correct?
Jul 21, 2015 #4 Masters2788 Mechanical Joined Apr 12, 2013 Messages 8 Location US I use the following stainless hardware when designing in accordance with ASME Section VIII, Div.1: 304 SS bolting = SA-193-B8 316 SS bolting = SA-193-B8M I have never used any of the designations you have listed for pressure vessel design. Upvote 0 Downvote
I use the following stainless hardware when designing in accordance with ASME Section VIII, Div.1: 304 SS bolting = SA-193-B8 316 SS bolting = SA-193-B8M I have never used any of the designations you have listed for pressure vessel design.