I'm in the process of doing a material analysis on some downhole products for the oil and gas industry. We thread the pieces of this component together, and it see's around 30ksi of pressure (which is balanced both inside and outside the tube). Our problem has been galling between these pieces of the assembly. Currently, we use 17-4 PH stainless due to its high yield strength and relatively good corrosion resistance in our application. Our problem is the thread galling between the two parts due to the stainless being the same material between the two mating surfaces.
My question concerns this Nitronic 60. Its great material for sure, has about the same yield strength as our current material at a level 3 HT. But its expensive stuff. I am curious though if I can use it on every other part, so that one thread is 17-4 and one is Nitronic. Will it have the same anti-galling properties, and not suffer from any galvanic corrosion (it has a short life so I wouldn't expect it), or other issues. 4140 would work as well in place of the 17-4, though its corrosion resistance is lower.
Part of the problem is we need a very tough material for the application. Occasionally these parts will see a one time stress of up to 100ksi (or higher in stress concentration areas). Therefore we can't use something like the Gall-Tough because its too weak.
Thanks.
My question concerns this Nitronic 60. Its great material for sure, has about the same yield strength as our current material at a level 3 HT. But its expensive stuff. I am curious though if I can use it on every other part, so that one thread is 17-4 and one is Nitronic. Will it have the same anti-galling properties, and not suffer from any galvanic corrosion (it has a short life so I wouldn't expect it), or other issues. 4140 would work as well in place of the 17-4, though its corrosion resistance is lower.
Part of the problem is we need a very tough material for the application. Occasionally these parts will see a one time stress of up to 100ksi (or higher in stress concentration areas). Therefore we can't use something like the Gall-Tough because its too weak.
Thanks.