I am looking at a process tank for a metal pre-treatment containing "fluoride compounds" in the range of 5-10%, phosphoric acid in the range of 1-5% and hexafluorotitanic acid in the range of
1-5%. The bath will consist of 5% of this chemical in DI water. Bath runs at ambient temperature and there is pump agitation. Would 304 suffice for this tank or is something more exotic required?
 
Replies continue below

Recommended for you

Although you did not mention volume required, I would consider a FRP tank or liner. Most pre-treatment tanks I have seen on various audits are now fiberglass.
 
Thanks, metengr--as a metallurgist, I always forget about the plastic option. Tank size will be around 700 gallons, BTW.
 