Yes. Passive stainless will promote the rapid consumption of the zinc, followed by the iron underneath it. It is best to use zinc coated fasteners (hot dipped galvanizing, zinc electroplating, or multilayer zinc flake coating) to join galvanized structures.
Regards,
Cory