Hi,
I am going to order a batch of SS321 piping (NPS14 sch.160 ; thk 35.71 mm) to use in estimated temperature of 500 C which is in sensitization susceptible range. Could anyone please suggest if I do require stabilization heat treatment after solution anneal ? If it is required (or recommended), please also help to suggest heat treatment conditions.
All comments are appreciated. Thank you.
I am going to order a batch of SS321 piping (NPS14 sch.160 ; thk 35.71 mm) to use in estimated temperature of 500 C which is in sensitization susceptible range. Could anyone please suggest if I do require stabilization heat treatment after solution anneal ? If it is required (or recommended), please also help to suggest heat treatment conditions.
All comments are appreciated. Thank you.