azertyuiop
Mechanical
Dear collegues ,
I want to check if the contractor is supplying my company an installation with the much more expensive SS316L materials that was demanded , and make sure he doesn't supply us cheaper SS304L materials instead (pharma applications).
How to check on this without damaging the delivered equipment/piping networks?
I have already used magnets to check if we are dealing here with stainless steel (the magnet doesn't clinch = SS) , but how to differentiate between the SS304L and SS316L variety ? Some tubing has SS316L inkinscriptions , but most (polished) parts are not tagged.
Expert advise needed.
regards.
I want to check if the contractor is supplying my company an installation with the much more expensive SS316L materials that was demanded , and make sure he doesn't supply us cheaper SS304L materials instead (pharma applications).
How to check on this without damaging the delivered equipment/piping networks?
I have already used magnets to check if we are dealing here with stainless steel (the magnet doesn't clinch = SS) , but how to differentiate between the SS304L and SS316L variety ? Some tubing has SS316L inkinscriptions , but most (polished) parts are not tagged.
Expert advise needed.
regards.