Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

How to achieve a uniform hardness value in the surface of polyurethane material

Status
Not open for further replies.

AlpanaSlo

Materials
Joined
Sep 11, 2023
Messages
1
Location
SI
Hello.
Our production producing Polyurethanes tubes for seals making by injection molding. Lately we faced the problem: Polyurethane tube after mixing in mold and subsequent curing has different surface hardness (difference can vary between ShA 80 and ShA 90). As far as seals are used in machinery with high requirements for phisical and mechanical characteristics, the hardness should vary for 1 or 2 units max.
Probably someone can suggest solutions to this problem?
We have already trued rheology/thixotropy agentsto make the polyurethane system more gomogeneous. Also we tried various catalysts to reduce curing time. Nothing has helped so far.
 
Post it in a chemical engineering forum.