I need to find the proper name of a spacer or wavvy type washer that you put in a socket weld fitting socket prior to welding. The purpose is to create a gap between the end of your pipe and the botton of the socket.The reason is so the weld does not become stressed or weakend because the of the expanding pipe will expand a lot more than the much heavier wall socket weld fitting. I have seen these rings in a publication more than once(can't find publication) but I cannot locate them on Google,Ask Jeeves and Thomas register, because I don't have there proper name I guess.