SS float level switch

Status
Not open for further replies.

chemilocha

Chemical
Joined
Nov 18, 2015
Messages
8
Location
NG
can we use SS float level switch in HCL tank ( 32-35% conc)?
 
chemilocha

No. 304 and 316 SS has minimal resistance to HCL and will suffer severe chloride corrosion. Some of the duplex stainless steels are somewhat resistant but still not a good choice. Why not try something like a HDPE float?

Regards
Ashtree
"Any water can be made potable if you filter it through enough money"
 
If the required level range can tolerate the % error in predicted density, why not use a remote sealed dp cell ? And if the vapor space is always close to or at atmospheric, further simplify this to a remote sealed PT to infer level?
 
A remote sealed PT or dp cell can be a cheaper alternative to avoid exotic materials that you would have to sue for a float switch..
 
georgeverghese

Probably the issue will be that they might be controlling directly with the float switch. It might be operating directly into a pump circuit, or a level alarm or whatever or it may be providing a digital input to a PLC.

If you change to a Pressure transducer this will be an analogue instrument (4-20ma or 0-10v or similar). This could require a change of wiring but might be able to be programmed into a PLC to stop/start/alarm etc at a particular tank level(ma or voltage level). However if it is working directly in a motor or alarm circuit there will need to be some sort of analogue to digital convertor to change an analogue to a switch function.

However following along your line though you can get units not unlike a PT which are in fact an adjustable pressure switch which may well do the job required. But many operators prefer a "float" switch because they can clearly see what is happening.

Regards
Ashtree
"Any water can be made potable if you filter it through enough money"
 