After forming Dish Head the SS 304 material became magnetic. I know Austenitic SS are not magnetic.
We doubted on the source of material and conucted re chemical analysis. The chemistry perfectly agrees with the material Spec SA 240- 304 not only that it perfectly matches the certificate.
Now why should the material which was non magnetic turn magnetic.
Had i performed Micro analysis before forming (Now also possible to perform since balance cut pieces of dish blank is availale) i would have seen Austenitic. What would i see in micro examination, Would i see Ferrite or martensite. If so how does this happen?
Would my ferrite scope show different reading in unformed plate and formed dish.
The problem with ferrite scope is that it shows various readings on the same plate.
After forming Dish Head the SS 304 material became magnetic. I know Austenitic SS are not magnetic.
We doubted on the source of material and conucted re chemical analysis. The chemistry perfectly agrees with the material Spec SA 240- 304 not only that it perfectly matches the certificate.
Now why should the material which was non magnetic turn magnetic.
Had i performed Micro analysis before forming (Now also possible to perform since balance cut pieces of dish blank is availale) i would have seen Austenitic. What would i see in micro examination, Would i see Ferrite or martensite. If so how does this happen?
Would my ferrite scope show different reading in unformed plate and formed dish.
The problem with ferrite scope is that it shows various readings on the same plate.