Is there a reliable acid spot test to determine if an alloy is predominantly Ti?

The best way to test something is to squeeze it, slowly, until it breaks!
 
Replies continue below

Recommended for you

I don't know of any straight acid test that will give you that information. A quick test is to spark it using a grinding wheel and if you get a shower of brilliant white parks you have a lot of Titanium. The only other material that makes this type display is Zirconium.

The two companies below make spot test kits for metals. I don't know if either has a teat for Ti.



Here is one that can sort Titanium alloys.

 
Can density measurement offer a clue instead?

Chocolates,men,coffee: are somethings liked better rich!!
(noticed in a coffee shop)
 
Great suggestion by Arun. How large are the parts? Density determination using the Archimedes principle is a simple test method.

Regards,

Cory