Hi everyone, I am currently having problems with mechanical seal failures on two Aurora Series 421 - Horizontal Multi Stage Split Case Pumps.
Sync speed of 3600RPM, ± 1000gpm
Size: 6x6 with an Impeller 11.315 trimmed down to 11.25in
by dealer in order to reduce amp draw
I would like to know how to proceed with troubleshooting this problem as there has been several seals that have blown (see attached pictures)
Is it possible to determine most likely cause from the pics or is there a standard pump seal failure checklist???
Thank you very much for the help.
I'll post more details as I get them.
Sync speed of 3600RPM, ± 1000gpm
Size: 6x6 with an Impeller 11.315 trimmed down to 11.25in
by dealer in order to reduce amp draw
I would like to know how to proceed with troubleshooting this problem as there has been several seals that have blown (see attached pictures)
Is it possible to determine most likely cause from the pics or is there a standard pump seal failure checklist???
Thank you very much for the help.
I'll post more details as I get them.