Hello,
In several websites for electric motor and pump repairs I found a shaft repair method called spiral welding technique
If anybody knows something regarding this method, please share...
Is it suitable for electric motors/pumps wоrn shafts? What is special?
Because what I know is to weld the shaft in lines parralel with the shaft, placed at 180o, to avoid shaft bending
In several websites for electric motor and pump repairs I found a shaft repair method called spiral welding technique
If anybody knows something regarding this method, please share...
Is it suitable for electric motors/pumps wоrn shafts? What is special?
Because what I know is to weld the shaft in lines parralel with the shaft, placed at 180o, to avoid shaft bending