Jun 14, 2015 #1 jlpinem Mechanical Joined Nov 19, 2014 Messages 2 Location ID Dear Friends I would like to know about the limitation of spiral welded pipe (API 5L X46)for cold bend application? is it alright to cold bend a spiral pipe? Thank you for your explanation Regards
Dear Friends I would like to know about the limitation of spiral welded pipe (API 5L X46)for cold bend application? is it alright to cold bend a spiral pipe? Thank you for your explanation Regards
Jun 14, 2015 #2 LittleInch Petroleum Joined Mar 27, 2013 Messages 23,123 Location GB There are no limitations. Yes it is alright. It is difficult to prove a negative, but there is no written limit another AFAIK. Remember - More details = better answers Also: If you get a response it's polite to respond to it. Upvote 0 Downvote
There are no limitations. Yes it is alright. It is difficult to prove a negative, but there is no written limit another AFAIK. Remember - More details = better answers Also: If you get a response it's polite to respond to it.