CSA Z245.1 specifies that ERW pipe must pass a root guided bend test in order to be qualified for sour service.
My question is: why is a root guided bend test necessary for sour service qualification?
Background: In the process of converting an existing Grade 359 Cat II pipeline for sour service, one of the cutouts met the microhardness requirements but snapped in half during the guided bend test...
My question is: why is a root guided bend test necessary for sour service qualification?
Background: In the process of converting an existing Grade 359 Cat II pipeline for sour service, one of the cutouts met the microhardness requirements but snapped in half during the guided bend test...