I am designing some injection molded parts to be made from abs/pc alloy. It is desireable to use glass fiber reinforcement. Is it possible to solvent bond these parts together? The stress on the joint is minimal.
 
Replies continue below

Recommended for you

Yes

It works better if some ABS or PC/ABS polymer is added to the solvent to increase viscosity and to "add material" to the joint as it evaporates.

Regards

eng-tips, by professional engineers for professional engineers
Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 
Thanks, Pat. I am used to solvent bonding neat resins only. I guess my real question is "Will the glass screw upo the bond?"
 
The glass reduces bond strength and leaves the bond interface depleted of resin, hence it is a bit more critical to replenish the resin at the interface.

The glass of course does not reinforce across the bond interface, but you already indicated the bond is not in a high stress area, so all should be OK

Regards

eng-tips, by professional engineers for professional engineers
Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 
Thanks for the expanded answer. This helps alot.
 