I am currently in the process of performing an assessment on an old underground pipe (approx 60 years) which has recently undergone In-Line-Inspection for the first time (High Res MFL).
With no previous inspection data to determine a corrosion rate, I have consulted API RP 581 (section 2.B.12 SOIL SIDE CORROSION) to estimate a corrosion rate and therefore determine which anomolies could reach critical size prior to the next inspection and therefore require repair, and to feed into the repair vs replace decision.
The pipeline is cathodically protected to an off potential more negative than -850 mV vs Cu/CuSO4, however the original coating was a coal tar enamel, and is known to be in poor condition. The on-potentials needed to maintain this level are such that further disbondment is expected. Therefore my main concern is areas where the CP is shielded by disbonded coating.
What i would like to understand is:
- How big a factor does soil corrosivity plays when the corrosion is occurring under disbonded coating?
- Can anyone suggest a factor I should use for those outlined in Table 2.B.12.3 – Soil Resistivity Adjustment of API RP 581 for this disbonded coating scenario
- Is anyone aware of research or guidance on estimating corrosion rates beneath disbonded CP coating
Thanks,
With no previous inspection data to determine a corrosion rate, I have consulted API RP 581 (section 2.B.12 SOIL SIDE CORROSION) to estimate a corrosion rate and therefore determine which anomolies could reach critical size prior to the next inspection and therefore require repair, and to feed into the repair vs replace decision.
The pipeline is cathodically protected to an off potential more negative than -850 mV vs Cu/CuSO4, however the original coating was a coal tar enamel, and is known to be in poor condition. The on-potentials needed to maintain this level are such that further disbondment is expected. Therefore my main concern is areas where the CP is shielded by disbonded coating.
What i would like to understand is:
- How big a factor does soil corrosivity plays when the corrosion is occurring under disbonded coating?
- Can anyone suggest a factor I should use for those outlined in Table 2.B.12.3 – Soil Resistivity Adjustment of API RP 581 for this disbonded coating scenario
- Is anyone aware of research or guidance on estimating corrosion rates beneath disbonded CP coating
Thanks,