Hello Gentle men,
for produced water service (in O&G production), corrosion is always a thing of concern. we have pipes 2" or less that needs to be buried (maybe some higher than 2")
1. If is a fair statement to state that corrosion is more of a worry in a socket weld than a threaded connection (I understand that crevice corrosion may be an issue only with socket weld, right?
2. with number 1 (corrosion) in mind, is it right to say that threading will be better if the pipe schedule is high enough or does it make any difference if it's socket welded or threaded?
3. If threaded is better, is it a bad practice to backweld the threaded connection as long as the exposted thread is covered by weldment to avoid stress rizers on the exposed threads?
DOES IT MAKE ANY DIFFERENCE IF
1. it's a natural gas serviec
2. or Oil piping
SUMMARY: is it better to have a good wall thickness, thread it and backweld (if need be) than to socket weld and stand the chance of suffering from corrosion in produced water, oil, and gas service piping?
THANK YOU VERY MUCH
As much as possible, do it right the first time...
for produced water service (in O&G production), corrosion is always a thing of concern. we have pipes 2" or less that needs to be buried (maybe some higher than 2")
1. If is a fair statement to state that corrosion is more of a worry in a socket weld than a threaded connection (I understand that crevice corrosion may be an issue only with socket weld, right?
2. with number 1 (corrosion) in mind, is it right to say that threading will be better if the pipe schedule is high enough or does it make any difference if it's socket welded or threaded?
3. If threaded is better, is it a bad practice to backweld the threaded connection as long as the exposted thread is covered by weldment to avoid stress rizers on the exposed threads?
DOES IT MAKE ANY DIFFERENCE IF
1. it's a natural gas serviec
2. or Oil piping
SUMMARY: is it better to have a good wall thickness, thread it and backweld (if need be) than to socket weld and stand the chance of suffering from corrosion in produced water, oil, and gas service piping?
THANK YOU VERY MUCH