Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

socket weld flange vs slip on flange

Status
Not open for further replies.

sftyvlv

Materials
May 7, 2007
28
What are the advantages or disadvantages of both? Why not just use socket weld flange for everything?
Sftyvlv







 
Replies continue below

Recommended for you

Socket-Weld fittings and flanges are NORMALLY used on 2" (DN 50mm) and smaller piping in non hygienic services and projects.

Slip-On flanges are NORMALLY used on low pressure, low temperature non-toxic services in sizes 3" (DN 80mm) and larger.

Exceptions may be made or required in both cases depending on specific situational conditions and/or Client specific directives.

What are the advantages? The answer to this is Safety and Cost.

Why not just use Socket-weld flanges in both cases? Have you tried to buy 12" (DN 300mm) Socket-Weld Flanges?
 
Slip-ons require the welding of TWO fillets. Relying on a single fillet weld at sizes beyond 2" is not permitted in most piping codes. So even if you could get larger socket welding flanges, you'd only be able to use them for non-hazardous and non-code services.
 
This question seems to come up at least once a month. Do a search on this forum and you'll get a list as long as your arm.

Only put off until tomorrow what you are willing to die having left undone. - Pablo Picasso
 
Slip-on flanges give alittle "fudge-factor" when your cutting them into an existing system.
 
Please regard to ASME B31.3 requirements:
For Slip-On Flanges: 308.2.1
For Socket Welding Flanges: 308.2.3 & 311.2.5
 