Gentlemen,
Our welding engineer is trying to increase the PWHT soaking time on production welds by 1.8 because some Inspector´s request.
Now a 3in. weld shall be PWHT at 1100 °F for 2.25 x 1.8 = 4.05 hrs instead of 2.25 hrs. per UCS-56-1.
From what I can read on the book and this forum that 80% of aggregate times at temperature is for test procedure qualification and not for production welds.
Any comment will be welcome.