Dear Guys,

Does any one suggest some brand name Soak film solution or commercial leak detection solution for vacuum test as per API 650 which i can buy online?

Thank you for your help.
z2175820051889_fef856e14ee9ce41e8d8612c68b7f7a5_bcw7cr.jpg
 
Replies continue below

Recommended for you

Be careful with bath soap, hand soap, party bubble mix, etc. Commercial solutions are more expensive but they are in many ways better. Low temperature tolerant, consistency in composition and performance between batches, and formulated for low corrosion when used on sensitive metals (aluminum, some stainless steels, some others), tested, certified, and accepted, etc.
 