SN curve for gray cast iron

Status
Not open for further replies.

mfinke

Mechanical
Nov 4, 2003
12
Dear all,

i´m looking for a SN - curve for the following material:

DIN: 0.6035
UNS: F13801
ASTM/AISI: A48, class 55B
UK: Grade 350

thank you in advance

regards

Matthias
 
Replies continue below

Recommended for you

There is a little data in the ASM publication " Atlas of Fatigue Curves" edited by H.E.Boyer - this references "Iron Castings Handbook" edited by C F Walton as the original source for the information.
 
You can also review this thread for additional information on GI castings ;
thread330-118025
 