Rejected welds based on kj/in. from actual values recorded during in-process welds.
So based on the WPS (not PQR) data below, can someone audit these numbers in accordance to API-1104 19th edition and maybe ASME Sect. IX (current)and tell me the allowable electrode diameter(s), travels speed(s) and kj/in. allowed per pass per code?
....................Electrode.............Dia .................AMP's .........VOLT...........Travel/Speed......KJ/IN
................................................MAX
ROOT.....SMAW.....E8010-P1........5/32"...DCRP....130 - 145.......25 to 28........10" to 14"......13.9 - 24.4
HOT.......SMAW.....E8010-P1........5/32"...DCRP....150 - 165.......26 to 29........10" to 15"......15.6 - 28.7
FILL.......SMAW.....E8010-P1.........5/32"...DCRP....140 - 145.......25 to 28........17" to 18"......11.7 - 14.3
or
FILL.......SMAW.....E8010-P1........3/16"....DCRP....145 - 180........27 to 30.........8" to 11".......21.4 - 40.5
CAP.......SMAW......E8010-P1.......3/16"... DCRP....130 - 165........28 to 30........12" to 15"......14.6 - 24.7
Rejected welds based on kj/in. from actual values recorded during in-process welds.
So based on the WPS (not PQR) data below, can someone audit these numbers in accordance to API-1104 19th edition and maybe ASME Sect. IX (current)and tell me the allowable electrode diameter(s), travels speed(s) and kj/in. allowed per pass per code?
....................Electrode.............Dia .................AMP's .........VOLT...........Travel/Speed......KJ/IN
................................................MAX
ROOT.....SMAW.....E8010-P1........5/32"...DCRP....130 - 145.......25 to 28........10" to 14"......13.9 - 24.4
HOT.......SMAW.....E8010-P1........5/32"...DCRP....150 - 165.......26 to 29........10" to 15"......15.6 - 28.7
FILL.......SMAW.....E8010-P1.........5/32"...DCRP....140 - 145.......25 to 28........17" to 18"......11.7 - 14.3
or
FILL.......SMAW.....E8010-P1........3/16"....DCRP....145 - 180........27 to 30.........8" to 11".......21.4 - 40.5
CAP.......SMAW......E8010-P1.......3/16"... DCRP....130 - 165........28 to 30........12" to 15"......14.6 - 24.7