twistedneck
Automotive
- Dec 13, 2005
- 81
Developing a small zinc casting using Zamak5, its not a precision or a thin walled casting, however extreme voids and porosity can result in a structural failure (yielding of the part).
What would be a good visual inspection method and standard to use? Of couse we have recommendations from our supplier, but i need help form the board here too.
Xray is not possible
Water weighing may work but the enviornment is very dirty
Cutting parts in half with a band saw is quite easy
Thank you
What would be a good visual inspection method and standard to use? Of couse we have recommendations from our supplier, but i need help form the board here too.
Xray is not possible
Water weighing may work but the enviornment is very dirty
Cutting parts in half with a band saw is quite easy
Thank you