I am working on a retro fit that has SJ167 joists specified in the drawings from 1954. I need the sectional properties to perform the checks I am working on, but due to the age I cannot find this information anywhere. Does anyone know where I can find this?
 
Replies continue below

Recommended for you

SJ167 - 16" deep joist
Moment capacity = 281,000 in-lbs (service capacity)
Max. End Reaction = 3,600 lbs
Span(ft) / TL capacity (plf)
27 / 257
28 / 239
29 / 223
30 / 208
31 / 195
32 / 183

You should buy the SJI 75 year Steel Joist Manual found here:

 