Any recommendations on reducing electrolytic hafnium pieces to around 0.5mm for an alloying application.

Ball Mill? Jaw Crusher?

Also I believe Hf is phosphoric and can ignite spontaneously in air when in powder form? Is there a safe way to do this?

Comments Please
 
Replies continue below

Recommended for you

SPEC mill... in argon might work... (SPEC stands for Specimen Preparation Extraction and Communution)

Or an autogeneous process....