Hi all

am after an equivalent for the Swedish steel grade SIS 1430.

I think its an old designation as the boiler it is from is about 30-35yrs old.

any advice would be greatly appreciated

cheers

Brund
 
Try a View for the C 22.8, 1.0460 P250GH -> 12024 Czech, SA 105-II, 1020
and/or EStE 285 1.1104 P275NL2 -> Fe 410-2KG Italy

hope this help.

Regards

Determ
 