Apr 18, 2011 #1 BrundLFly Marine/Ocean Joined Jun 21, 2010 Messages 8 Location GB Hi all am after an equivalent for the Swedish steel grade SIS 1430. I think its an old designation as the boiler it is from is about 30-35yrs old. any advice would be greatly appreciated cheers Brund
Hi all am after an equivalent for the Swedish steel grade SIS 1430. I think its an old designation as the boiler it is from is about 30-35yrs old. any advice would be greatly appreciated cheers Brund
Apr 18, 2011 #2 Determ Materials Joined Jun 8, 2009 Messages 11 Location DE Try a View for the C 22.8, 1.0460 P250GH -> 12024 Czech, SA 105-II, 1020 and/or EStE 285 1.1104 P275NL2 -> Fe 410-2KG Italy hope this help. Regards Determ Upvote 0 Downvote
Try a View for the C 22.8, 1.0460 P250GH -> 12024 Czech, SA 105-II, 1020 and/or EStE 285 1.1104 P275NL2 -> Fe 410-2KG Italy hope this help. Regards Determ