Hi,
`
I`m working on a small research related to internal cathodic protection of oil-water separator tanks(on-shore) operating under higher temperatures(~80 C). Anybody has some hint on how to simulate(simplified but 3D, in matlab for example) polarization spreading when using impressed current protection?

Thanks in advance,
Cleber
 
Replies continue below

Recommended for you

I don't know how to simulate it, but I'm really interested in your research. I've had a bunch of "experts" (I guess that means they're from out of town) claim that there is no way that impressed current can possibly have any impact on internal corrosion. Conceptually, I disagree with them, but data is sorely lacking on either side.

Where are you doing your research and will it be published?

David
 
The experts probably came from a different planet but that's another story. Impressed current is a little unwieldy because: a) it will require a dedicated vessel entry point; b) there is a lot of metalwork, deflector plates, mist mats etc etc, hanging around inside complicating space; c) it will require monitoring which is no easy matter in operation; and d) there is scope to blow off the internal coating with poor control. Generally, the industry will go with a good coating and sacrificial anodes simply changing them out at vessel inspections - it's by far the simplest way to go and it does work.

For researching 'polarisation spreading', I can only recommend producing a simulated vessel bottom with a simulated oil water mixture and simply mapping the potential with a reference electrode probe.

Steve Jones