Just eyeballing the basic properties, silicon looks like a candidate for a high preformance reinforcement. (Strength maybe 7000 MPa, E about 150 GPa, density 2330 kg/m3.) However, I can't find any reference to its use as such (and no references to any sort of fibres of silicon).
Anyone aware of use as reinforcement (maybe in a non-fibrous form)? And anyone have any idea why it's not used as such?