Is Silicant rubber sealant OK at -40C?
(the standard industrial stuff)
Thanks
 
Depends what type of silicone sealant you are using. The one we spec is good for -60 C. Most aircraft grade sealants are good to at least -40 C.

-Reidh
 
what does it say on the container??
 
Thanks for the replies, just found some local that withstands -60
 
Hi.
How many types of silicon rubber are there for water radiator gasket use in vehicle?
Best Regards
 
Three:

Group 1 are the ones that work properly

Group 3 are the ones that don't work at all

Group 2 are the ones that are between Groups 1 and 3.

You will probably end up using Group 2



Cheers

Greg Locock

Please see FAQ731-376 for tips on how to make the best use of Eng-Tips.
 

Since this is the "Automotive engineering - other topics" forum, I assume that you're using it on an engine and that engine may be gasoline (?)
If so, it's important to only use silicone sealing materials that are specifically intended for engines as any free silicone that manages to get into the oil or fuel systems can initiate a degradation or even failure of the HEGO.


Bill
 
No, it will be used just to stop a nylon cover dropping of a nut.
For info the silicone I got is from Beal (UK) Ltd. It is called Trust Seal R.T.V silicone seal. Colour : Black. Temp Range : -60 deg C to +250 Deg C
 