Dear all,
I have a large ductile iron casting ~250lbs with a wall thickness of 1 inch in resin bonded sand.
I got shrinkage issues that I can't seem to get rid off.
Chemistry :
C: 3.82
Si: 2.65
Mn .449
S 0.0108
Cu 0.0765
Mg 0.0319
Cr 0.0262
Pour Temp is 2590F.
Nodularity is great.
Any ideas?