This photo shows a repair in a carpark slab on ground. Apparently a water hydrant line failed under this point so the builder saw cut a hole, fixed the pipe and did this repair.
You can see there are radiating cracks out from the hole. I am assuming this is due to a release of shrinkage tension in the mesh when the hole was cut out of it, however would like your expert opinions!
I don't have details of the original leak and symptoms.