We are currently reburbishing a customers gearbox not manufactured by ourselves.
The situation is we have a shaft onto which a gearwheel is shrunk on.
The trouble is that the shaft has a 1:32 taper. What I need to know is info about the torque it will be able to transmit and also, how to install the gear. I have a feeling it is oil injection but could it be forced on with hydraulic rams.
Thanks