Johnae;
For the WPS to be qualified in accordance with Section IX of the ASME B&PV Code, the welding processes on the WPS must be supported by the welding processes used in the PQR.
So, the PQR that was generated for this WPS must have the GMAW and the SMAW processes qualified. Keep in mind that you can have multiple PQR's support a WPS.