Does anyone (Will ?) have references for the need to shotpeen machined fittings ?
I am looking for myself, but I guess here is a good source of info.
We're being "challenged" to come up with a justification beyond "industry practice" when we call up shotpeening on fittings machined from thick billets, to address the corrosion concern (not for fatigue benefit, we keep that in our back pocket !).
another day in paradise, or is paradise one day closer ?
Does anyone (Will ?) have references for the need to shotpeen machined fittings ?
I am looking for myself, but I guess here is a good source of info.
We're being "challenged" to come up with a justification beyond "industry practice" when we call up shotpeening on fittings machined from thick billets, to address the corrosion concern (not for fatigue benefit, we keep that in our back pocket !).
another day in paradise, or is paradise one day closer ?