Jan 19, 2005 #1 LENEW Mechanical Joined Nov 7, 2003 Messages 19 Location CA Hi guys, I have a short flat belt: 1. 10 ft long; 2. 48 in wide; 3. 450 fpm for belt speed; 4. 12 inches for pulley diameter Considering the speed and length, what kind of splice you think will be good? if use mechanical type, any bad effects? Lenew
Hi guys, I have a short flat belt: 1. 10 ft long; 2. 48 in wide; 3. 450 fpm for belt speed; 4. 12 inches for pulley diameter Considering the speed and length, what kind of splice you think will be good? if use mechanical type, any bad effects? Lenew
Jan 19, 2005 #2 M MintJulep Mechanical Joined Jun 12, 2003 Messages 10,242 Location JP Duct tape. Providing more detailed information on the application will probably result in better answers than that. Upvote 0 Downvote
Duct tape. Providing more detailed information on the application will probably result in better answers than that.
Jan 19, 2005 Thread starter #3 LENEW Mechanical Joined Nov 7, 2003 Messages 19 Location CA The belt will be used to move dirt or earch. The density is between 70-120 lb/cu ft. That is surface application not underground mining. Is that enough to understand the situation? Lenew Upvote 0 Downvote
The belt will be used to move dirt or earch. The density is between 70-120 lb/cu ft. That is surface application not underground mining. Is that enough to understand the situation? Lenew
Jan 19, 2005 #4 M MintJulep Mechanical Joined Jun 12, 2003 Messages 10,242 Location JP Belt material is rubber? fabric? PVC? Metal mesh? Fiberglass? Some combination of those? Is it supported between the rollers? On what? Have a look at http://www.habasitabt.com/ Upvote 0 Downvote
Belt material is rubber? fabric? PVC? Metal mesh? Fiberglass? Some combination of those? Is it supported between the rollers? On what? Have a look at http://www.habasitabt.com/