bernardoporta
Structural
The case we are facing involves three columns whose anchor bolts were misplaced resulting in a situation where the top of the anchor bolt is below the top of the nut. Is plug welding into the nut an acceptable fix? or alternatively Is welding the nut to the base plate a good fix?
Thank you all for your opinions
Thank you all for your opinions