Hello,

ASME B31.8/4 has field cold bend information. ASME B16.49 has factory induction bend information. What ASME or US applicable specification has Factory Cold bend information?

Thank you.
 
Replies continue below

Recommended for you

What sort of radius are you looking at?

The hot bend spec is still valid, just don't heat the pipe.

Remember - More details = better answers
Also: If you get a response it's polite to respond to it.
 
Then just use B31 4 or 31.8.

The term "field" is immaterial.

I've never heard of "shop" cold bends at 30 to 40 D before. A cold bend is a cold bend irrespective of where it happens, in the field (usually); in factory (unusual) or in your kitchen (the plumber). Did that help?

Remember - More details = better answers
Also: If you get a response it's polite to respond to it.
 
Yes, it did help. Some clients I work with ask for a combination of shop and field cold bends, though I agree it's quite unusual.
 
I once had to get two 10D cold bends made (don't ask), and that involved ramming sand inside the pipe whilst bending it.

Now that was a factory cold bend.

It's the only one Ive done in 40 yrs of doing this sort of thing

Remember - More details = better answers