I am going to run a PQR joining 625 (solution annealed) to itself using NiCrMo-3 filler. GTAW in the root and deposit 6mm of weld metal. Then GMAW-Pulse for the remainder. The test plates will be 40mm thick and double U Preps will be machined at 60 deg included.
What shielding gas is recommended for GMAW-Pulse process? I believe 100% Ar can be used but would a He blend be better for penetration and avoiding lack of fusion defects and toe wetting?