I'm working on cost-reduction project. I like to know more on sheetmetal fabrication to analyze sequesnce of operation & to negotiate with vendors. Would any of advise me with reference meaterials, videos & slides etc.,

Thanks,
Santy
 
passanthosh,

What kind of sheet metal work are you doing?

Get a copy of Product Design for Manufacture and Assembly by Boothroyd, Dewhurst and Knight. There is a section on sheet metal there. There is all sorts of other useful stuff.

As noted above, you definitely should talk to your vendors.

Critter.gif
JHG
 
Try Architectural Sheet Metal Manual from SMACNA....
 
You're not going to get anything but basic stuff out of a book. Schedule a tour as a potential customer to several sheetmetal fab shops, as others have suggested. Eyes and ears open, don't be afraid to ask question, don't be afraid to pick up parts and look them over on the way through the shop. You'll learn more in 2 hours than in a month of book reading.

Sheetmetal assemblies can be complex, and quite precise. Do some reading on the British sten gun of WWII. Genius. And developed by people not afraid to take a chance and try something totally against the convention of the day.

You mentioned sequence of operations. This all depends on your part. There are so many operations that can be done, and it also depends on the capability and the equipment of the vendor.
 
"There are so many operations that can be done, and it also depends on the capability and the equipment of the vendor. "

Exactly, that's why you probably want to try and find out what capabilities your likely vendors have, and if they can meet your functional needs.

If you need something your obvious vendors can't give you then you either need to find another vendor or find another way of 'skinning the cat'.

For instance, I fine tuned some vent holes on a low volume enclosure to suit our preferred vendors tooling. It was a case where functional requirements could be met in several ways and I was able to find an easy/cheap one.

Posting guidelines faq731-376 (probably not aimed specifically at you)
What is Engineering anyway: faq1088-1484
 
passanthosh (Mechanical)

drawoh (Mechanical) asked you what kind of sheet metal work you are doing.
You are not really going to get a sensible answer to your questions until you get more specific,and tell us what your line of work is.
That's why most of the posters are saying talk to your vendors because right now it is the only constructive answer we can give you.
B.E.
 
Running a sheet metal Shop is pretty much the same as any metal working plant
1 Engineer the product - Layout the piece you are working on to obtain the most economical cut of material - Check your inventory for something close not assigned to a project - Layout the lines of cut and Break or roll and them check it against your engineering - measure twice cut once - Take the unit to the break or roll and shape the piece - then check your engineering sketch for dimention s
and weld procedures - weld it up -
Have a good day
 
Hi,
Below is a typical Sheetmetal Fabrication shop process list.
These are in a process order but not necessarily so
Each process may have several sub-processes


•Cad - Flat Pattern Development
•CNC Programming
•Pattern layout
•Manual Fabrication
•Guillotine
•Turret Punch
•Back-cut/Guillotine
•Power Press
•Deburr
•Drill/Tap/Csk
•Press Brake
•Roll/Form
•Insert Setting
•Spot-weld
•Welding
•Pretreatment
•Finishing
•Outwork
•Inspection/Q/A
•Re-work ;-)
•Dispatch/Stores

 